P-7001

Passivation compound, free of nitric-acid, for use on stainless steel parts. Use at 120-140F for best results. DO NOT USE ABOVE 160F. Time and exposure is dependent upon application and alloy. User should validate their specific process results with copper sulfate test of substrate passivated.